Pyrotek F-24 Dense Machinable Board

Category Polymer , Thermoset , Filled/Reinforced Thermoset
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek F-24 Dense Machinable Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
F-24 is a high temperature resin material that is reinforced with fiberglass. Abrasion resistant, it is used for hot glass handling applications.ApplicationsDonut rollers for glass Guide rails Wear pads Machined insulators AdvantagesAbrasion resistant Excellent heat resistance Non-marking to glass Economical Easily machined Good physical strength Excellent wear resistance Good shock resistance Information provided by Pyrotek.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.0 MPa
2760 psi
Flexural Strength 31.0 MPa
4500 psi
Compressive Strength 76.0 MPa
11000 psi
Shear Strength 52.0 MPa
7540 psi
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
Thermal Properties Metric English Comments
Thermal Conductivity 0.0900 W/m-K
0.625 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 470 °C
878 °F
Continuous