Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), Extrusion Grade
Manufacturer Quadrant Engineering Plastics Products
Trade Name Duratron® PEI
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it ideal for high strength/high heat applications, and those requiring consistent dielectric properties over a wide frequency range. It is hydrolysis resistant, highly resistant to acidic solutions and capable of withstanding multiple autoclaving cycles.Duratron® U1000 is FDA and USP Class VI compliant. FDA compliant colors of Ultem are also available on a custom basis. Duratron® U1000 commonly is machined into parts for reusable medical devices, analytical instrumentation, electrical/electronic insulators and a variety of structural components requiring high strength and rigidity at elevated temperatures.Data provided by Quadrant Engineering Plastic Products from tests on stock shapes and parts produced by Quadrant EPP.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Water Absorption 0.25 %
0.25 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 1.25 %
1.25 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell M 112
112
ASTM D785
Hardness, Rockwell R 125
125
ASTM D785
Hardness, Shore D 86
86
ASTM D2240
Tensile Strength 117 MPa
17000 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Tensile Modulus 3.45 GPa
500 ksi
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Compressive Strength 152 MPa
22000 psi
10% Def.; ASTM D695
Compressive Modulus 3.31 GPa
480 ksi
ASTM D695
Shear Strength 103 MPa
15000 psi
ASTM D732
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.42
0.42
Dry vs. Steel; QTM55007
K (wear) Factor 5840 x 10-8 mm³/N-M
2900 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.06568 MPa-m/sec
1875 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 55.8 µm/m-°C

@Temperature -40.0 - 149 °C
31.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.177 W/m-K
1.23 BTU-in/hr-ft²-°F
ASTM F433
Maximum Service Temperature, Air 171 °C
340 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
ASTM D648
Glass Transition Temp, Tg 210 °C
410 °F
ASTM D3418
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Dielectric Constant 3.15

@Frequency 1e+6 Hz
3.15

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 32.7 kV/mm
830 kV/in
Short Term; ASTM D149
Dissipation Factor 0.0013

@Frequency 1e+6 Hz
0.0013

@Frequency 1e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA Yes
Yes
NSF Yes
Yes
STD 51, Natural Only
USDA Yes
Yes
USP Class VI Yes
Yes
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Unacceptable
Unacceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Limited
Limited
Hydrocarbons - Aromatic Unacceptable
Unacceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Descriptive Properties Value Comments
Color Natural and black
Machinability 3
1-10, 1=Easier to Machine
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved