Material Notes:
Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant composition. The acetal copolymer is more resistant against hydrolysis, strong alkalis and thermal-oxidative degradation than the acetal homopolymer High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stability (low water absorption) Good sliding properties and wear resistance Excellent machinability Good electrical insulating and dielectric properties Physiologically inert (most grades are suitable for food contact) Not self-extinguishing
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %
0.20 %
50% RH
Water Absorption at Saturation 0.80 %
0.80 %
Outgassing - Total Mass Loss 0.34 %
0.34 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 84
84
ISO 2039-2
Hardness, Shore D 79
79
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Tensile Strength 66.0 MPa
9570 psi
at Yield; ISO 527-1/-2
Elongation at Break 50 %
50 %
ISO 527-1/-2
Elongation at Yield 20 %
20 %
ISO 527-1/-2
Tensile Modulus 2.80 GPa
406 ksi
ISO 527-1/-2
Flexural Strength 91.0 MPa
13200 psi
Flexural Modulus 2.66 GPa
386 ksi
Compressive Strength 23.0 MPa

@Strain 1 %
3340 psi

@Strain 1 %
ISO 604
40.0 MPa

@Strain 2 %
5800 psi

@Strain 2 %
ISO 604
72.0 MPa

@Strain 5 %
10400 psi

@Strain 5 %
ISO 604
K Factor (ISO) 45 µm/km
45 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.30 - 0.45
0.30 - 0.45
Limiting Pressure Velocity 0.100 MPa-m/sec
2860 psi-ft/min
at 1 m/s unlubricated
0.160 MPa-m/sec
4570 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 125 µm/m-°C

@Temperature 23.0 - 100 °C
69.4 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.310 W/m-K
2.15 BTU-in/hr-ft²-°F
Melting Point 165 °C
329 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 100 °C
212 °F
Continuous; 20,000 h
115 °C
239 °F
Continuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Oxygen Index 15 %
15 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency >=100000 Hz
3.8

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
Dissipation Factor 0.0030

@Frequency 100000 Hz
0.0030

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy Yes
Yes
Only natural
European Food 1935/2004 Yes
Yes
only natural
FDA Yes
Yes
only natural
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable