Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ertalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an excellent wear resistance. It also allows higher max. service temperatures High mechanical strength, stiffness, hardness and toughness Good fatigue resistance High mechanical damping ability Good sliding properties Excellent wear resistance Good electrical insulating properties Good resistance to high energy radiation (gamma- and X-rays) Good machinability
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH
Water Absorption at Saturation 5.5 %
5.5 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 76
76
ISO 2039-2
Hardness, Shore D 80
80
Ball Indentation Hardness 165 MPa
23900 psi
ISO 2039-1
Tensile Strength 85.0 MPa
12300 psi
at Yield; ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 5.00 GPa
725 ksi
ISO 527-1/-2
Compressive Strength 43.0 MPa

@Strain 1 %
6240 psi

@Strain 1 %
ISO 604
77.0 MPa

@Strain 2 %
11200 psi

@Strain 2 %
ISO 604
112 MPa

@Strain 5 %
16200 psi

@Strain 5 %
ISO 604
K Factor (ISO) 11 µm/km
11 µm/km
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.25 - 0.40
0.25 - 0.40
Limiting Pressure Velocity 0.120 MPa-m/sec
3430 psi-ft/min
at 1 m/s unlubricated
0.180 MPa-m/sec
5140 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 23.0 - 100 °C
33.3 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Melting Point 260 °C
500 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 110 °C
230 °F
Continuous; 20,000 h
120 °C
248 °F
Continuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 3.9

@Frequency >=100000 Hz
3.9

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm
686 kV/in
Dissipation Factor 0.012

@Frequency 100000 Hz
0.012

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 475 V
475 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable