Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ketron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unreinforced PEEK, the carbon fibres considerably reduce thermal expansion and provide 3.5 times higher thermal conductivity – dissipating heat from the bearing surface faster, improving bearing life and pressure-velocity capabilities Very high maximum allowable service temperature in air (250 °C continuously, up to 310 °C for short periods of time) High mechanical strength, stiffness and creep resistance, also at elevated temperatures Excellent chemical and hydrolysis resistance Excellent wear & frictional behaviour Very good dimensional stability Excellent resistance to high energy radiation (gamma- and X-rays) Inherent low flammability and very low levels of smoke evolution during combustion
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.16 %
0.16 %
50% RH
Water Absorption at Saturation 0.35 %
0.35 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102
102
ISO 2039-2
Hardness, Shore D 90
90
Ball Indentation Hardness 310 MPa
45000 psi
ISO 2039-1
Tensile Strength 144 MPa
20900 psi
at Break (NYP); ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
ISO 527-1/-2
Tensile Modulus 9.20 GPa
1330 ksi
ISO 527-1/-2
Flexural Strength 220 MPa
31900 psi
Compressive Strength 69.0 MPa

@Strain 1 %
10000 psi

@Strain 1 %
ISO 604
125 MPa

@Strain 2 %
18100 psi

@Strain 2 %
ISO 604
170 MPa

@Strain 5 %
24700 psi

@Strain 5 %
ISO 604
K Factor (ISO) 2.0 µm/km
2.0 µm/km
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.20 - 0.30
0.20 - 0.30
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C

@Temperature 23.0 - 100 °C
13.9 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.920 W/m-K
6.38 BTU-in/hr-ft²-°F
Melting Point 340 °C
644 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 40 %
40 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity <= 1e+05
<= 1e+05
IEC 60093
Surface Resistivity per Square <= 1e+05
<= 1e+05
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative Yes
Yes
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Users viewing this material also viewed the following: