Quadrant EPP Ketron® CM HPV PEEK (1331) Compression Molded High Pressure Velocity Polyetherether Ketone

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ketron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ketron® CM HPV PEEK (1331) Compression Molded High Pressure Velocity Polyetherether Ketone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc

@Temperature 22.8 °C
1.44 g/cc

@Temperature 73.0 °F
ASTM D792
Water Absorption 0.070 %
0.070 %
IMMERSION; 24HRS; ASTM D570 2
Mechanical Properties Metric English Comments
Tensile Strength 54.5 MPa
7900 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 3.65 GPa

@Temperature 22.8 °C
530 ksi

@Temperature 73.0 °F
ASTM D638
Flexural Strength 89.6 MPa

@Temperature 22.8 °C
13000 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 4.83 GPa

@Temperature 22.8 °C
700 ksi

@Temperature 73.0 °F
ASTM D790
Compressive Strength 138 MPa

@Strain 10.0 %,
Temperature 22.8 °C
20000 psi

@Strain 10.0 %,
Temperature 73.0 °F
ASTM D625
Coefficient of Friction, Dynamic 0.20
0.20
QTM 55007
Limiting Pressure Velocity 1.23 MPa-m/sec
35000 psi-ft/min
(with 4:1 safety factor applied); QTM 55010
Thermal Properties Metric English Comments
Melting Point 340 °C
644 °F
ASTM D3418