Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Ketron® LSG GF30 PEEK + glass fibres, LSG grade, extruded (ISO Data)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ketron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ketron® LSG GF30 PEEK + glass fibres, LSG grade, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Within its portfolio of Life Science Grade Engineering Plastic Products - specifically developed for applications in the medical, pharmaceutical and biotechnology industries - Quadrant offers KETRON PEEK-CLASSIXä LSG white, KETRON PEEK-CA30 LSG, KETRON PEEK-GF30 LSG blue (RAL 5019) and KETRON PEEK LSG natural / black biocompatible engineering plastic stock shapes for machining with certified USP Class VI and ISO 10993 compliance Very high maximum allowable service temperature in air (250 °C continuously, up to 310 °C for short periods of time) High mechanical strength, stiffness and creep resistance, also at elevated temperatures Excellent chemical and hydrolysis resistance Excellent wear & frictional behaviour Very good dimensional stability Excellent resistance to high energy radiation (gamma- and X-rays) Inherent low flammability and very low levels of smoke evolution during combustion
Mechanical Properties Metric English Comments
K Factor (ISO) 7.0 µm/km
7.0 µm/km
Coefficient of Friction, Dynamic 0.30 - 0.45
0.30 - 0.45
Compliance Properties Metric English Comments
3A-Dairy No
No
USP Class VI Yes
Yes
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Users viewing this material also viewed the following: