Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Nylon
Manufacturer Quadrant Engineering Plastics Products
Trade Name Nylatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 6.0 %
6.0 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 68.3 MPa
9900 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 3.21 GPa
465 ksi
ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 3.62 GPa
525 ksi
ASTM D790
Compressive Strength 93.1 MPa
13500 psi
10% Def.; ASTM D695
Compressive Modulus 2.28 GPa
330 ksi
ASTM D695
Shear Strength 64.1 MPa
9300 psi
ASTM D732
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.14
0.14
Dry vs. Steel; QTM55007
K (wear) Factor 145 x 10-8 mm³/N-M
72.0 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 101 µm/m-°C

@Temperature -40.0 - 149 °C
56.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Melting Point 216 °C
420 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 104 °C
220 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
ASTM D648
Flammability, UL94 HB
HB
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+13 ohm
1.00e+13 ohm
EOS/ESD S11.11
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Machinability 2
1-10, 1=Easier to Machine