Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Quadrant LSG PC extruded (ISO Data)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Extruded
Manufacturer Quadrant Engineering Plastics Products
Trade Name Quadrant LSG
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Quadrant LSG PC extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Within its portfolio of Life Science Grade Engineering Plastic Products - specifically developed for applications in the medical, pharmaceutical and biotechnology industries - Quadrant offers QUADRANT LSG PC natural biocompatible engineering plastic stock shapes for machining with certified USP Class VI and ISO 10993 compliance High mechanical strength Good creep resistance Very high impact strength, even at low temperatures Stiffness retention over a wide range of temperatures Very good dimensional stability (very low water absorption and low coefficient of linear thermal expansion) Natural colour (clear, translucent) Good electrical insulating and dielectric properties Physiologically inert (suitable for food contact) Economical thermal performance
Mechanical Properties Metric English Comments
K Factor (ISO) 60 µm/km
60 µm/km
Coefficient of Friction, Dynamic 0.50 - 0.60
0.50 - 0.60
Compliance Properties Metric English Comments
3A-Dairy No
No
USP Class VI Yes
Yes
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Unacceptable
Unacceptable
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Unacceptable
Unacceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Users viewing this material also viewed the following: