Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Quadrant Engineering Plastics Products
Trade Name Semitron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Quadrant Engineering Plastic ProductsThis PEEK based static dissipative material provides a dissipative range of 10E+6 - 10E+9 ohms/sq. Semitron® ESd 480 is very dimensionally stable, making it ideal for critical test fixture applications. Its exceptional chemical resistance makes it well suited for use in wafer handling and other structural applications in wet process tools where static dissipation is important. Like all Quadrant Semitron® ESd materials, Semitron ESd480 is not subject to dielectric breakdown.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Water Absorption 0.18 %
0.18 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 1.65 %
1.65 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell M 107
107
ASTM D785
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength 100 MPa
14500 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Tensile Modulus 6.48 GPa
940 ksi
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Compressive Strength 183 MPa
26500 psi
10% Def.; ASTM D695
Compressive Modulus 3.93 GPa
570 ksi
ASTM D695
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.20
0.20
Dry vs. Steel; QTM55007
K (wear) Factor 403 x 10-8 mm³/N-M
200 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 1.26 MPa-m/sec
36000 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C

@Temperature -40.0 - 149 °C
17.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Melting Point 340 °C
644 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 246 °C
475 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+6 - 1.00e+9 ohm
1.00e+6 - 1.00e+9 ohm
EOS/ESD S11.11
Dielectric Constant 10.9

@Frequency 1e+6 Hz
10.9

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.518

@Frequency 1e+6 Hz
0.518

@Frequency 1e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative Yes
Yes
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Machinability 4
1-10, 1=Easier to Machine