Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer Quadrant Engineering Plastics Products
Trade Name Semitron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (low coefficient of linear thermal expansion and small water absorption), ideal for handling equipment in the electrical/electronic or semiconductor industries Surface resistivity: 104 - 106 ohms/sq. Thermal performance to 210 °C (410 °F) Low stress for tight tolerance machining High strength and stiffness
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.60 %
0.60 %
50% RH
Water Absorption at Saturation 1.1 %
1.1 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 115
115
ISO 2039-2
Hardness, Shore D 85
85
Tensile Strength 62.0 MPa
8990 psi
at Break (NYP); ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
ISO 527-1/-2
Tensile Modulus 5.85 GPa
848 ksi
ISO 527-1/-2
Flexural Strength 80.0 MPa
11600 psi
Compressive Strength 44.0 MPa

@Strain 1 %
6380 psi

@Strain 1 %
ISO 604
76.0 MPa

@Strain 2 %
11000 psi

@Strain 2 %
ISO 604
114 MPa

@Strain 5 %
16500 psi

@Strain 5 %
ISO 604
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179-1/1eA
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 23.0 - 100 °C
22.2 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C
338 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-1/-2
Glass Transition Temp, Tg 215 °C
419 °F
DSC, 20°C/min.; ISO 11357-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 47 %
47 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 10000 - 1.0e+6 ohm-cm
10000 - 1.0e+6 ohm-cm
IEC 60093
Surface Resistivity per Square 10000 - 1.0e+6 ohm
10000 - 1.0e+6 ohm
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Unacceptable
Unacceptable
Conductive / Static Dissipative Yes
Yes
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Limited
Limited
Hydrocarbons - Aromatic Unacceptable
Unacceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Users viewing this material also viewed the following: