Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data)

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE/ECTFE, Molded/Extruded
Manufacturer Quadrant Engineering Plastics Products
Trade Name Symalit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistance. Thermal stability in the range -76 °C up to +160 °C / -105 °F up to + 356 °F Excellent chemical resistance against highly concentrated chemicals, even for a broad range of alcalines (up to pH 14) Low permeability to liquids, gases and vapors. High elongation at break Excellent impact resistance Good resistance to stress cracking, even with caustic solutions, chlorine and alkaline areas Excellent weather proof and radiation proof Low coefficient of thermal expansion
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.040 %
0.040 %
50% RH
Water Absorption at Saturation <= 0.10 %
<= 0.10 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ISO 2039-2
Hardness, Shore D 70
70
Ball Indentation Hardness 65.0 MPa
9430 psi
ISO 2039-1
Tensile Strength 30.0 MPa
4350 psi
at Yield; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 1.60 GPa
232 ksi
ISO 527-1/-2
Flexural Strength 47.0 MPa
6820 psi
Compressive Strength 14.5 MPa

@Strain 1 %
2100 psi

@Strain 1 %
ISO 604
26.0 MPa

@Strain 2 %
3770 psi

@Strain 2 %
ISO 604
33.0 MPa

@Strain 5 %
4790 psi

@Strain 5 %
ISO 604
K Factor (ISO) 1100 µm/km
1100 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 18.0 J/cm²
85.7 ft-lb/in²
Partial Break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35 - 0.45
0.35 - 0.45
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C

@Temperature 23.0 - 100 °C
66.7 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.150 W/m-K
1.04 BTU-in/hr-ft²-°F
Melting Point 240 °C
464 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 160 °C
320 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 52 %
52 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 2.5

@Frequency >=100000 Hz
2.5

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm
660 kV/in
Dissipation Factor 0.0010

@Frequency 100000 Hz
0.0010

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Copyright © lookpolymers.com All Rights Reserved