Material Notes:
Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to high-energy radiation (considerably better than most other fluoropolymers). Resistance to chemicals (up to pH 11) Dimensional stability from - 40 °C to + 150 °C (-40 °F to + 302 °F) Extremely good mechanical characteristics Excellent abrasion resistance Excellent ageing stability Resistance to UV-, ß- and gamma -rays High dielectric and piezoelectric values
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.050 %
0.050 %
50% RH
Water Absorption at Saturation <= 0.10 %
<= 0.10 %
Outgassing - Total Mass Loss 0.050 %
0.050 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 78
78
ISO 2039-2
Hardness, Shore D 78
78
Ball Indentation Hardness 110 MPa
16000 psi
ISO 2039-1
Tensile Strength 60.0 MPa
8700 psi
at Yield; ISO 527-1/-2
Elongation at Break 30 %
30 %
ISO 527-1/-2
Elongation at Yield 9.0 %
9.0 %
ISO 527-1/-2
Tensile Modulus 2.20 GPa
319 ksi
ISO 527-1/-2
Flexural Strength 80.0 MPa
11600 psi
Compressive Strength 20.0 MPa

@Strain 1 %
2900 psi

@Strain 1 %
ISO 604
36.0 MPa

@Strain 2 %
5220 psi

@Strain 2 %
ISO 604
62.0 MPa

@Strain 5 %
8990 psi

@Strain 5 %
ISO 604
K Factor (ISO) 455 µm/km
455 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35 - 0.45
0.35 - 0.45
Limiting Pressure Velocity 0.100 MPa-m/sec
2860 psi-ft/min
at 1 m/s unlubricated
0.160 MPa-m/sec
4570 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 190 µm/m-°C

@Temperature 23.0 - 100 °C
106 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Melting Point 175 °C
347 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C
302 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 44 %
44 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 7.4

@Frequency >=100000 Hz
7.4

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
Dissipation Factor 0.025

@Frequency 100000 Hz
0.025

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy Yes
Yes
Only natural
European Food 1935/2004 Yes
Yes
FDA Yes
Yes
only natural
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable