Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Quadrant Engineering Plastics Products
Trade Name TIVAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufacturing paper with high abrasive filler content. High load, High-speed, abrasive applications Reduces noise Self-lubricating Wear-resistant Corrosion-resistant No moisture absorption
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183-1
Water Absorption <= 0.10 %
<= 0.10 %
96 hr; ISO 62
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
50% RH
Water Absorption at Saturation <= 0.10 %
<= 0.10 %
ISO 62
Outgassing - Total Mass Loss 0.14 %
0.14 %
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Ball Indentation Hardness 33.0 MPa
4790 psi
ISO 2039-1
Tensile Strength 18.0 MPa
2610 psi
at Yield; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 15 %
15 %
ISO 527-1/-2
Tensile Modulus 0.750 GPa
109 ksi
ISO 527-1/-2
Flexural Strength 17.0 MPa
2470 psi
Compressive Strength 7.00 MPa

@Strain 1 %
1020 psi

@Strain 1 %
ISO 604
11.0 MPa

@Strain 2 %
1600 psi

@Strain 2 %
ISO 604
17.5 MPa

@Strain 5 %
2540 psi

@Strain 5 %
ISO 604
K Factor (ISO) 4.0 µm/km
4.0 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 10.5 J/cm²
50.0 ft-lb/in²
Partial Break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.20 - 0.35
0.20 - 0.35
Sand Slurry 75
75
Limiting Pressure Velocity 0.0500 MPa-m/sec
1430 psi-ft/min
at 1 m/s unlubricated
0.0800 MPa-m/sec
2280 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 23.0 - 100 °C
111 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
Melting Point 135 °C
275 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Oxygen Index <= 20 %
<= 20 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+12 ohm
>= 1.0e+12 ohm
IEC 60093
Dielectric Strength 45.0 kV/mm
1140 kV/in
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Continuous Sunlight Limited
Limited
Hot Water / Steam Unacceptable
Unacceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Limited
Limited
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable