Qualchem Danamid FCP-40 Polyamide 6, 40% Carbon Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid FCP-40 Polyamide 6, 40% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Filled with milled carbon fiber, antistatic and conductiveInformation provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
DIN 53479
Filler Content 40 %
40 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
50 mm/min; ISO 527-1,2
Elongation at Break 4.0 %
4.0 %
ISO 527-1,2
Charpy Impact Unnotched 3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
DIN 53482
Processing Properties Metric English Comments
Moisture Content 1.5 - 1.8 %
1.5 - 1.8 %
DIN 53714