Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC

Category Polymer , Thermoset , Composite SMC , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Quantum Composites
Trade Name Lytex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance and low density. It utilizes a 12K Tow carbon fiber reinforcement.Form = SheetColor = BlackGlass Fiber Content = 50 to 55%Information provided by Quantum Composites.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 138 MPa
20000 psi
ASTM D638
Flexural Strength 310 MPa
45000 psi
ASTM D790
Flexural Modulus 27.6 GPa
4000 ksi
ASTM D790
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 5.50 µm/m-°C
3.06 µin/in-°F
TMA
Thermal Conductivity 0.450 W/m-K
3.12 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °C
347 °F
300 °C
572 °F
Deflection Temperature, Load not specified; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 129 - 166 °C
265 - 330 °F
Mold Temperature
Cure Time 5.00 - 10.0 min
0.0833 - 0.167 hour
Shelf Life 6.00 Month

@Temperature -12.2 °C
6.00 Month

@Temperature 10.0 °F
Descriptive Properties Value Comments
Fiber Length (in) 0.5
Carbon