Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Vinyl Ester , Vinyl Ester Sheet Molding Compound
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QC-8100 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and corrosion resistance. Form and Colors = Rolled Sheet, Natural/Black. Glass Fiber Length = 1 inch.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 213 MPa
30900 psi
ASTM D638
Flexural Yield Strength 413 MPa
59900 psi
ASTM D790
Flexural Modulus 15.8 GPa
2290 ksi
ASTM D790
Compressive Yield Strength 246 MPa
35700 psi
ASTM D695
Izod Impact, Notched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 145 °C
293 °F
DMA, ASTM D4065
Shrinkage <= 0.0010 %
<= 0.0010 %
ASTM D955
Processing Properties Metric English Comments
Processing Temperature 127 - 160 °C
261 - 320 °F
Mold temperature