Information provided by Quantum Advanced Engineering Plastics
Physical Properties Metric English Comments
Specific Gravity 1.78 g/cc
1.78 g/cc
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Water Absorption at Saturation 0.050 %
0.050 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ASTM D785
Hardness, Rockwell R 84
84
ASTM D785
Hardness, Shore D 77
77
ASTM 2240
Tensile Strength 48.3 MPa
7000 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Tensile Modulus 1.72 GPa
250 ksi
ASTM D638
Flexural Strength 20.7 MPa
3000 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Compressive Strength 72.4 MPa
10500 psi
ASTM D695
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Coefficient of Friction 0.58
0.58
Thermal Properties Metric English Comments
CTE, linear 119 µm/m-°C
66.0 µin/in-°F
ASTM D696
Thermal Conductivity 0.108 W/m-K
0.750 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 168 °C
335 °F
ASTM D3417
Maximum Service Temperature, Air 138 °C
280 °F
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
ASTM D257
Dielectric Constant 8.35

@Frequency 1.00e+6 Hz
8.35

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 63.0 kV/mm
1600 kV/in
ASTM D149
Dissipation Factor 0.060

@Frequency 1.00e+6 Hz
0.060

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
FDA Compliance yes