RTP Company ESD C 700 A Low Density Polyethylene (LDPE), ESD Protection - Electrically Conductive

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer RTP Company
Trade Name ESD
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company ESD C 700 A Low Density Polyethylene (LDPE), ESD Protection - Electrically Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D 792
Linear Mold Shrinkage 0.0170 - 0.0220 cm/cm

@Thickness 3.20 mm
0.0170 - 0.0220 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.3 MPa
1500 psi
ASTM D 638
Elongation at Break >= 10.0 %
>= 10.0 %
ASTM D 638
Tensile Modulus 0.345 GPa
50.0 ksi
ASTM D 638
Flexural Strength 13.8 MPa
2000 psi
ASTM D 790
Flexural Modulus 0.345 GPa
50.0 ksi
ASTM D 790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.20 mm
8.00 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB

@Thickness 3.20 mm
NB

@Thickness 0.126 in
ASTM D 4812
Electrical Properties Metric English Comments
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ASTM D 257
Surface Resistance <= 1e+05
<= 1e+05
ESD STM11.11
Surface Resistivity per Square <= 1.00e+6 ohm
<= 1.00e+6 ohm
ASTM D 257; ESD STM11.11
Static Decay <= 2.00 sec
<= 2.00 sec
MIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 193 - 232 °C
380 - 450 °F
Mold Temperature 21.1 - 65.6 °C
70.0 - 150 °F
Drying Temperature 79.4 °C

@Time 7200 sec
175 °F

@Time 2.00 hour
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi