RTP Company RTP 1300 MG 50 SI 2  Polyphenylene Sulfide (PPS) Milled Glass 50% - Silicone 2%  

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1300 MG 50 SI 2  Polyphenylene Sulfide (PPS) Milled Glass 50% - Silicone 2%  .pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Milled Glass 50% - Silicone 2%Comments:Milled GlassSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.73 g/cc
1.73 g/cc
ASTM D792
Water Absorption 0.020 %
0.020 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
0.0030 cm/cm

@Thickness 6.35 mm
0.0030 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Ultimate 103 MPa
15000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Modulus of Elasticity 13.8 GPa
2000 ksi
ASTM D638
Flexural Yield Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 12.4 GPa
1800 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm

@Thickness 3.17 mm
6.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 266 °C
510 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 288 - 321 °C
550 - 610 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments
Color Natural/Black