Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D 792
Water Absorption 0.54 %

@Temperature 23.0 °C,
Time 86400 sec
0.54 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage 0.0070 cm/cm

@Thickness 3.20 mm
0.0070 in/in

@Thickness 0.126 in
ASTM D 955
Melt Flow 80 g/10 min

@Load 2.16 kg,
Temperature 385 °C
80 g/10 min

@Load 4.76 lb,
Temperature 725 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.7 MPa
12000 psi
ASTM D 638
Elongation at Break 30 %
30 %
ASTM D 638
Tensile Modulus 2.69 GPa
390 ksi
ASTM D 638
Flexural Strength 111 MPa
16100 psi
ASTM D 790
Flexural Modulus 2.90 GPa
420 ksi
ASTM D 790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.20 mm
1.30 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 48.6 µm/m-°C
27.0 µin/in-°F
E 831
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
398 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
ASTM D 257
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
Dry; ASTM D 150
Dielectric Strength 15.0 kV/mm
380 kV/in
in oil; S/T; ASTM D 149
Dissipation Factor 0.0056

@Frequency 1.00e+6 Hz
0.0056

@Frequency 1.00e+6 Hz
Dry; ASTM D 150
Processing Properties Metric English Comments
Melt Temperature 343 - 377 °C
650 - 710 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Drying Temperature 149 °C

@Time 21600 sec
300 °F

@Time 6.00 hour
Moisture Content 0.040 %
0.040 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi