Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D 792
Water Absorption 0.37 %
0.37 %
24 hrs @ 23°C; ASTM D 570
Melt Flow 22 - 28 g/10 min

@Load 5.00 kg,
Temperature 365 °C
22 - 28 g/10 min

@Load 11.0 lb,
Temperature 689 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 69.6 MPa
10100 psi
ASTM D 638
Elongation at Break 90 %
90 %
ASTM D 638
Tensile Modulus 2.34 GPa
340 ksi
ASTM D 638
Flexural Strength 91.0 MPa
13200 psi
ASTM D 790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D 790
Izod Impact, Notched 6.94 J/cm

@Thickness 3.17 mm
13.0 ft-lb/in

@Thickness 0.125 in
D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
408 °F
ASTM D 648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
ASTM D 257
Processing Properties Metric English Comments
Melt Temperature 343 - 388 °C
650 - 730 °F
Mold Temperature 138 - 163 °C
280 - 325 °F
Drying Temperature 149 °C
300 °F
Dry Time 6 hour
6 hour
Moisture Content 0.040 %
0.040 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 138 MPa
10000 - 20000 psi
Copyright © lookpolymers.com All Rights Reserved