Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1404 N L  Polyethersulfone (PES) Glass Fiber 25% - Lubricated - High Viscosity &n

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 30%Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1404 N L  Polyethersulfone (PES) Glass Fiber 25% - Lubricated - High Viscosity &n.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Fiber 25% - Lubricated - High ViscosityComments:Glass FiberHigh ViscosityLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Filler Content 25 %
25 %
Water Absorption 0.35 %
0.35 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 138 MPa
20000 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
Modulus of Elasticity 8.27 GPa
1200 ksi
ASTM D638
Flexural Yield Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Compressive Yield Strength 141 MPa
20500 psi
ASTM D695
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.94 J/cm

@Thickness 3.17 mm
13.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 214 °C
417 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
Processing Properties Metric English Comments
Processing Temperature 343 - 366 °C
650 - 690 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Descriptive Properties Value Comments
Color Natural/Black