Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 1499 P X 125056 A Polyphenyl Sulfone (PPSU) Stainless Steel Fiber - EMI/RFI Shielding

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer RTP Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 1499 P X 125056 A Polyphenyl Sulfone (PPSU) Stainless Steel Fiber - EMI/RFI Shielding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D 792
Additive Loading 10 %
10 %
Primary Additive
Linear Mold Shrinkage 0.0040 - 0.0090 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0090 in/in

@Thickness 0.126 in
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.9 MPa
10000 psi
ASTM D 638
Elongation at Break >= 10 %
>= 10 %
ASTM D 638
Tensile Modulus 2.34 GPa
340 ksi
ASTM D 638
Flexural Strength 89.6 MPa
13000 psi
ASTM D 790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D 790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB

@Thickness 3.20 mm
NB

@Thickness 0.126 in
ASTM D 4812
Electrical Properties Metric English Comments
Volume Resistivity <= 100 ohm-cm
<= 100 ohm-cm
ASTM D 257
Surface Resistance <= 1000 ohm
<= 1000 ohm
ESD STM11.11
Surface Resistivity per Square <= 10000 ohm
<= 10000 ohm
ASTM D 257
Static Decay <= 2.0 sec
<= 2.0 sec
FTMS101C; 4046.1
Processing Properties Metric English Comments
Melt Temperature 343 - 377 °C
650 - 710 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Drying Temperature 149 °C

@Time 21600 sec
300 °F

@Time 6.00 hour
Moisture Content 0.040 %
0.040 %
Dew Point -31.7 °C
-25.0 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi