Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 2800 B-55A HF Thermoplastic Polyolefin Elastomer (TEO) High Flow

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 2800 B-55A HF Thermoplastic Polyolefin Elastomer (TEO) High Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 55.0
55.0
10 s delay; ASTM D 2240
Tensile Strength at Break 4.14 MPa

@Thickness 3.20 mm
600 psi

@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
Tensile Strength, Yield 1.83 MPa

@Strain 100 %,
Thickness 3.20 mm
265 psi

@Strain 100 %,
Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
Elongation at Break 450 %

@Thickness 3.20 mm
450 %

@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
Tear Strength 19.3 kN/m
110 pli
Die C; ASTM D 624
Processing Properties Metric English Comments
Melt Temperature 182 - 210 °C
360 - 410 °F
Mold Temperature 15.6 - 65.6 °C
60.0 - 150 °F
Drying Temperature 79.4 °C

@Time 7200 sec
175 °F

@Time 2.00 hour
Moisture Content 0.0300 %
0.0300 %
Dew Point -17.8 °C
0.000 °F
Injection Pressure 82.7 - 124 MPa
12000 - 18000 psi