Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 287D  Nylon 6/12 (PA 6/12) Carbon Fiber 40%  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Carbon Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 287D  Nylon 6/12 (PA 6/12) Carbon Fiber 40%  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon Fiber 40%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Filler Content 40 %
40 %
Water Absorption 0.22 %
0.22 %
24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
0.0020 cm/cm

@Thickness 6.35 mm
0.0020 in/in

@Thickness 0.250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 228 MPa
33000 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ASTM D638
Modulus of Elasticity 27.6 GPa
4000 ksi
ASTM D638
Flexural Yield Strength 345 MPa
50000 psi
ASTM D790
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 8.54 J/cm

@Thickness 3.17 mm
16.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 227 °C
440 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 0.100 ohm-cm
0.100 ohm-cm
ASTM D257
Surface Resistance 1e+05
1e+05
ASTM D257
Processing Properties Metric English Comments
Processing Temperature 252 - 279 °C
485 - 535 °F
Mold Temperature 60.0 - 93.3 °C
140 - 200 °F
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Descriptive Properties Value Comments
Color Natural/Black