Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.35 g/cc | 0.0488 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 3.17 mm |
0.010 in/in @Thickness 0.125 in |
ASTM D955 |
0.014 cm/cm @Thickness 6.35 mm |
0.014 in/in @Thickness 0.250 in |
ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Elongation at Break | 6.5 % | 6.5 % | ASTM D638 |
Tensile Modulus | 3.10 GPa | 450 ksi | ASTM D638 |
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
Izod Impact, Notched | 1.30 J/cm @Thickness 3.17 mm |
2.44 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Izod Impact, Unnotched | 6.40 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |