Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RTP Company RTP 687 HB Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber - UL94 HB

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 40% Carbon Fiber Filled
Manufacturer RTP Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RTP Company RTP 687 HB Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber - UL94 HB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The RTP 680 HB are carbon fiber reinforced ABS. These materials offer a good combination of physical properties, stiffness and the ability to be fabricated to close dimensional tolerances.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D 792
Filler Content 40 %
40 %
Primary Additive
Water Absorption 0.14 %
0.14 %
24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.00010 - 0.00050 cm/cm

@Thickness 3.17 mm
0.00010 - 0.00050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D 785
Tensile Strength at Break 131 MPa
19000 psi
ASTM D 638
Elongation at Break 1.2 %
1.2 %
ASTM D 638
Tensile Modulus 23.4 GPa
3400 ksi
ASTM D 638
Flexural Strength 193 MPa
28000 psi
ASTM D 790
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
D 256
Izod Impact, Unnotched 3.20 J/cm

@Thickness 3.17 mm
6.00 ft-lb/in

@Thickness 0.125 in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
245 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
240 °F
ASTM D 648
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
Electrical Properties Metric English Comments
Volume Resistivity <= 1e+05
<= 1e+05
ASTM D 257
Processing Properties Metric English Comments
Melt Temperature 204 - 238 °C
400 - 460 °F
Mold Temperature 62.8 - 85.0 °C
145 - 185 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 2 hour
2 hour
Moisture Content 0.10 %
0.10 %
Dew Point -17.8 °C
0.000 °F
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Copyright © lookpolymers.com All Rights Reserved