Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler |
Manufacturer | RTP Company |
Trade Name | |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | RTP Company RTP PP 30 GF FR0 NAT Polypropylene (PP), Glass Fiber - Flame Retardant - Value Product - UL94.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D 792 |
Additive Loading | 30 % | 30 % | Primary Additive |
Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm @Thickness 3.17 mm |
0.0010 - 0.0030 in/in @Thickness 0.125 in |
ASTM D 955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 105 | 105 | ASTM D 785 |
Tensile Strength at Break | 68.9 MPa | 10000 psi | ASTM D 638 |
Elongation at Break | 2.0 - 4.0 % | 2.0 - 4.0 % | ASTM D 638 |
Tensile Modulus | 7.58 GPa | 1100 ksi | ASTM D 638 |
Flexural Strength | 110 MPa | 16000 psi | ASTM D 790 |
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D 790 |
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D 256 |
Izod Impact, Unnotched | 5.34 J/cm @Thickness 3.17 mm |
10.0 ft-lb/in @Thickness 0.125 in |
ASTM D 4812 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 154 °C | 310 °F | ASTM D 648 |
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 290 °F | ASTM D 648 |
Flammability, UL94 | V-0 @Thickness 0.7937 mm |
V-0 @Thickness 0.03125 in |
|
V-0 @Thickness 3.17 mm |
V-0 @Thickness 0.125 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D 257 |
Dielectric Constant | 3.3 @Frequency 1.00e+6 Hz |
3.3 @Frequency 1.00e+6 Hz |
Dry; ASTM D 150 |
Dielectric Strength | 17.7 kV/mm | 450 kV/in | short term, in oil; ASTM D 149 |
Dissipation Factor | 0.0030 @Frequency 1.00e+6 Hz |
0.0030 @Frequency 1.00e+6 Hz |
Dry; ASTM D 150 |
Arc Resistance | 85 sec | 85 sec | ASTM D 495 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 191 - 232 °C | 375 - 450 °F | |
Mold Temperature | 32.2 - 65.6 °C | 90.0 - 150 °F | |
Drying Temperature | 79.4 °C @Time 7200 sec |
175 °F @Time 2.00 hour |
|
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi |