Radici Heraflex® A 57-41-90 TPS-SEBS Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Radici Group Plastics
Trade Name Heraflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Heraflex® A 57-41-90 TPS-SEBS Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shore hardness: 57A (3s)Good price / compression set ratioApplication examples: sealing for spoutsInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57