Material Notes:
PA6 flame retardant injection molding grade. Halogen and phosphorus free. Natural color. Suitable for monofilament extrusion.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 28 %
28 %
Tensile Modulus 2.45 GPa
355 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.220 J/cm²

@Temperature -30.0 °C
1.05 ft-lb/in²

@Temperature -22.0 °F
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V