Material Notes:
PA6 Self-extinguishing without halogen or phosphorousInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527-1/2
Elongation at Break 30 %
30 %
ISO 527-1/2
Elongation at Yield 4.0 %
4.0 %
ISO 524-1/2
Tensile Modulus 3.35 GPa
486 ksi
ISO 527-1/2
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 2.80 GPa
406 ksi
ISO 178
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75/2Af
Vicat Softening Point 195 °C
383 °F
ISO 306
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in