Radici Radilon® A RCV3015 RKC Nylon 66-GF30

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A RCV3015 RKC Nylon 66-GF30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive cooling liquid resistant PA66-GF30 grade designed to be processed by GIT technology.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 123 MPa
17800 psi
ISO 527
Elongation at Break 2.3 %
2.3 %
ISO 527
Tensile Modulus 6.65 GPa
965 ksi
ISO 527
Flexural Modulus 6.10 GPa
885 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in