Material Notes:
Glass-fiber reinforced with heat and hydrolysis resistanceInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 185 MPa
26800 psi
ISO 527-1/2
Elongation at Break 3.6 %
3.6 %
ISO 527-1/2
Tensile Modulus 10.55 GPa
1530 ksi
ISO 527-1/2
Flexural Strength 270 MPa
39200 psi
ISO 178
Flexural Modulus 8.45 GPa
1230 ksi
ISO 178
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ISO 75/2Af
Vicat Softening Point 255 °C
491 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in