Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® CST 38FL (cond.) Nylon 6/66

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® CST 38FL (cond.) Nylon 6/66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 11 %
11 %
Tensile Modulus 1.25 GPa
181 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.290 J/cm²

@Temperature -30.0 °C
1.38 ft-lb/in²

@Temperature -22.0 °F
15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: