Material Notes:
Medium high viscosityInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527-1/2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/2
Elongation at Yield 3.5 %
3.5 %
ISO 524-1/2
Tensile Modulus 3.10 GPa
450 ksi
ISO 527-1/2
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 2.45 GPa
355 ksi
ISO 178
Charpy Impact, Notched 0.680 J/cm²
3.24 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75/2Af
Vicat Softening Point 195 °C
383 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in