Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Raschig Group RESINOL® 400 EPF Phenolic

Category Polymer , Thermoset , Phenolic
Manufacturer Raschig Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Raschig Group RESINOL® 400 EPF Phenolic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS)Processing: Injection and compression molding Applications: CommutatorsInformation provided by Raschig Group
Physical Properties Metric English Comments
Specific Gravity 1.85 - 1.95 g/cc
1.85 - 1.95 g/cc
ISO 1183
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
ISO 60
Water Absorption <= 0.200 %

@Temperature 23.0 °C,
Time 86400 sec
<= 0.200 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.00300 - 0.00500 cm/cm
0.00300 - 0.00500 in/in
Injection and Compression; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Compression; ISO 527
100 - 120 MPa
14500 - 17400 psi
Injection; ISO 527
Modulus of Elasticity 7.00 - 9.00 GPa
1020 - 1310 ksi
Injection and Compression; ISO 527
Flexural Strength 120 - 140 MPa
17400 - 20300 psi
Compression; ISO 178
200 - 220 MPa
29000 - 31900 psi
Injection; ISO 178
Flexural Modulus 16.0 - 18.0 GPa
2320 - 2610 ksi
Compression; ISO 178
18.0 - 22.0 GPa
2610 - 3190 ksi
Injection; ISO 178
Compressive Strength 250 - 300 MPa
36300 - 43500 psi
ISO 604
Charpy Impact Unnotched 0.600 - 0.800 J/cm²
2.86 - 3.81 ft-lb/in²
Compression; ISO 179/1eU
1.00 - 1.20 J/cm²
4.76 - 5.71 ft-lb/in²
Injection; ISO 179/1eU
Charpy Impact, Notched 0.200 - 0.300 J/cm²
0.952 - 1.43 ft-lb/in²
Compression; ISO 179/1eA
0.300 - 0.500 J/cm²
1.43 - 2.38 ft-lb/in²
Injection; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C

@Temperature 50.0 - 150 °C
8.33 - 11.1 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Thermal Conductivity 0.400 - 0.600 W/m-K
2.78 - 4.16 BTU-in/hr-ft²-°F
ASTM E1461
Maximum Service Temperature, Air 150 °C

@Time 7.20e+7 sec
302 °F

@Time 20000 hour
IEC 60216/T1
230 °C

@Time <=180000 sec
446 °F

@Time <=50.0 hour
IEC 60216/T1
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C
>= 392 °F
ISO 75-A
Deflection Temperature at 8.0 MPa 160 - 180 °C
320 - 356 °F
ISO 75-C
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage <= 0.0500 %

@Temperature 110 °C,
Time 605000 sec
<= 0.0500 %

@Temperature 230 °F,
Time 168 hour
Post shrinkage; ISO 2577
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 - 1.00e+13 ohm-cm
1.00e+12 - 1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 - 1.00e+11 ohm
1.00e+10 - 1.00e+11 ohm
IEC 60093
Dielectric Constant 4.00 - 6.00

@Frequency 1.00e+6 Hz
4.00 - 6.00

@Frequency 1.00e+6 Hz
IEC 60250
6.00 - 8.00

@Frequency 100 Hz
6.00 - 8.00

@Frequency 100 Hz
IEC 60250
Dielectric Strength 20.0 - 30.0 kV/mm
508 - 762 kV/in
IEC 60243-1
Dissipation Factor 0.0200 - 0.0300

@Frequency 1.00e+6 Hz
0.0200 - 0.0300

@Frequency 1.00e+6 Hz
IEC 60250
0.100 - 0.200

@Frequency 100 Hz
0.100 - 0.200

@Frequency 100 Hz
IEC 60250
Arc Resistance 180 - 240 sec
180 - 240 sec
ASTM D495
Comparative Tracking Index >= 175 V
>= 175 V
IEC 60112
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 20.0 - 30.0 °C
12.0 Month

@Temperature 68.0 - 86.0 °F
Descriptive Properties Value Comments
Glow wire flammability test 960/1
IEC 60695 2-12
Glow wire ignitability test 960/1
IEC 60695 2-13
Water Absorption <20 mg
24 hr, 23°C; ISO 62