Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Echo® RPPC 20/2 BK Recycled Polypropylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Echo®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Echo® RPPC 20/2 BK Recycled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copolymer Polypropylene, Unreinforced, 20 MFI, 2 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 28 %
28 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 0.951 GPa
138 ksi
ASTM D638
Flexural Strength 23.0 MPa
3340 psi
ASTM D790
Flexural Modulus 1.034 GPa
150.0 ksi
1% Secant; ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
ASTM D648
Vicat Softening Point 68.0 °C
154 °F
50N; ASTM D1525