Ravago Manufacturing Americas Echo® RPPC 30/2 BK Recycled Polypropylene

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Echo®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Echo® RPPC 30/2 BK Recycled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copolymer Polypropylene, Unreinforced, 30 MFI, 2 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Flexural Modulus 1.135 GPa
164.6 ksi
ASTM D790
Izod Impact, Notched 1.06 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
1.99 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648