Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Enviramid™ N2300THL BK Post Consumer Recycle Nylon 6

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Enviramid™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Enviramid™ N2300THL BK Post Consumer Recycle Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 1.6 %
1.6 %
Saturation, Immersed; ASTM D570
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm

@Thickness 3.17 mm
0.015 - 0.019 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7970 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.099 GPa
304.5 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256