Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Enviramid™ N2335HL BK Nylon 6

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Filled, Impact Grade
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Enviramid™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Enviramid™ N2335HL BK Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Filler: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedContains Recycled ContentRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 148 MPa
21500 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Flexural Strength 170 MPa
24700 psi
ASTM D790
Flexural Modulus 7.52 GPa
1090 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
Unannealed; ASTM D648