Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hybrid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec and Ravago.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Melt Flow 25 g/10 min

@Load 5.00 kg,
Temperature 260 °C
25 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Flexural Yield Strength 72.4 MPa
10500 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
73°F, 0.125 in; ASTM D256
4.81 J/cm

@Temperature -50.0 °C
9.00 ft-lb/in

@Temperature -58.0 °F
0.125 in; ASTM D256
5.34 J/cm

@Temperature -40.0 °C
10.0 ft-lb/in

@Temperature -40.0 °F
0.125 in; ASTM D256
6.14 J/cm

@Temperature -30.0 °C
11.5 ft-lb/in

@Temperature -22.0 °F
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.9 °C
192 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 243 - 266 °C
470 - 510 °F
Middle Barrel Temperature 249 - 271 °C
480 - 520 °F
Front Barrel Temperature 254 - 277 °C
490 - 530 °F
Nozzle Temperature 254 - 271 °C
490 - 520 °F
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Drying Temperature 110 °C
230 °F
Dry Time 4 - 6 hour
4 - 6 hour
Shot Size 50 - 80 %
50 - 80 %
Screw Speed 50 - 80 rpm
50 - 80 rpm
Descriptive Properties Value Comments
Injection Rate Moderate
Copyright © lookpolymers.com All Rights Reserved