Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hybrid S493 ABS + Polycarbonate Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate (PC)
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hybrid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hybrid S493 ABS + Polycarbonate Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium Impact, Enhanced Heat PerformanceEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 13 g/10 min

@Load 10.0 kg,
Temperature 220 °C
13 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.747 MPa
6199.9 psi
ASTM D638
Flexural Strength 77.22 MPa
11200 psi
ASTM D790
Flexural Modulus 2.516 GPa
364.9 ksi
ASTM D790
Izod Impact, Notched 2.5093 J/cm
4.7009 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Flammability, UL94 HB
HB