Material Notes:
Available in North America Features: Flame Retardant, Halogen Free and High Flow RoHS Compliant Form: PelletsInformation provided by Ravago
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 25 g/10 min

@Load 1.20 kg,
Temperature 300 °C
25 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0590 in
UL 94
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
UL94