Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (Cond)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (Cond)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
DAM; ASTM D792
Water Absorption 0.50 %
0.50 %
24 hrs, DAM; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
0.125 in, DAM; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 83
83
ASTM D785
Tensile Strength at Break 103 MPa
15000 psi
ASTM D638
Flexural Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
0.0591 in, BK
HB
HB
0.118 in, BK
Processing Properties Metric English Comments
Melt Temperature 282 - 299 °C
540 - 570 °F
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.18 %
0.18 %
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Screw Speed 40 - 120 rpm
40 - 120 rpm