Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hysun™ 678 ASA

Category Polymer , Thermoplastic , ASA Polymer
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hysun™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hysun™ 678 ASA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Availibility: North America Features: Good Impact Resistance and High Heat Resistance RoHS Compliant Forms: PelletsInformation provided by Ravago.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
0.125 in; ASTM D955
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.3 MPa
7000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 70.3 MPa
10200 psi
ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 3.20 J/cm
6.00 ft-lb/in
73°F, 0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
Unannealed (0.250 in); ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
217 °F
Unannealed (0.250 in); ASTM D648
Vicat Softening Point 104 °C
220 °F
Rate A; ASTM D1525