Ravago Manufacturing Americas Hysun™ A3525 ASA+PC

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hysun™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hysun™ A3525 ASA+PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Melt Flow 25 g/10 min

@Load 5.00 kg,
Temperature 250 °C
25 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 84.1 MPa
12200 psi
ASTM D790
Flexural Modulus 2.65 GPa
385 ksi
ASTM D790
Izod Impact, Notched 5.02 J/cm
9.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 101 °C
213 °F
Unannealed; ASTM D648