Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

RedEye On Demand Polycarbonate High Impact Strength & Temperature Resistant for Rapid Prototyping

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer RedEye On Demand
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF RedEye On Demand Polycarbonate High Impact Strength & Temperature Resistant for Rapid Prototyping.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate (PC) is an actual industrial-grade thermoplastic that is impact-resistant and structurally strong. PC parts are built with a layered manufacturing process utilizing Fused Deposition Modeling (FDM) technology, often used in rapid prototyping. Polycarbonate parts produced with FDM are dimensionally stable and will not shrink, warp, or absorb moisture. This high-performance engineering material can handle greater forces and loads than ABS material and is ideal for functional prototypes and end-use parts.ApplicationsDue to its high impact strength and compressive strength, Polycarbonate is used in a myriad of applications including cell phones, business equipment, computer products, manufacturing fixtures, and a wide variety of consumer products, such as appliances. Parts built from PC can also be used as masters for RTV molds and vacuum forming, vacuum metallization and electroplating.In a rapid manufacturing application, Polycarbonate can be used to create actual production parts in lieu of injection molding for short-run production. Rapid (or layered) manufacturing provides multiple benefits:High design iterations – while in production the design engineer has the freedom to modify geometry’s on the fly which cannot be done once you have committed to toolingBridge manufacturing – with rapid manufactured parts, production can begin while permanent tooling is on orderJigs and Fixtures to be used on manufacturing/production linesFor those manufacturers who practice lean manufacturing techniques or who maintain just-in-time inventories, RM can conserve cash flowAlpha and beta product releases – manufacturers can produce accurate, durable products even in the earliest stages of production
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
Tensile Strength, Yield 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Flexural Yield Strength 97.0 MPa
14100 psi
ASTM D790
Flexural Modulus 2.137 GPa
310.0 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 127 °C
261 °F
HDT unspecified pressure; ASTM D648
Glass Transition Temp, Tg 161 °C
322 °F
DMA (SYSS)
Flammability, UL94 V-2

@Thickness 1.10 mm
V-2

@Thickness 0.0433 in
Electrical Properties Metric English Comments
Dielectric Constant 3.17

@Frequency 6.00e+7 Hz
3.17

@Frequency 6.00e+7 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm
381 kV/in
IEC 60112