Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Reliance Industries Relene B31101 Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Relene B31101 Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Steel pipe coating base High Density Polyethylene resin. Characteristics:broad molecular weight distribution, good melting strength, excellent toughness/ESCR, and good cut through/abrasion resistance. Information provided by Reliance Industries
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 400 hour
>= 400 hour
F<sub>0</sub>; ASTM D1693/B
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
ASTM D3895
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.25
2.25
ASTM D150
Dissipation Factor 0.000040
0.000040
ASTM D150