Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Reliance Industries Relene B56003 Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Reliance Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Relene B56003 Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Relene B56003 is a High Density Polyethylene grade suitable for general purpose extrusion blow molding applications. Articles blown from this grade exhibit good stiffness. The resin offers good melt strength, ESCR and impact resistance and typically is used for packing of oils, vanaspati, and general purpose containers. Information provided by Reliance Industries
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
Melt Flow 0.30 g/10 min

@Load 2.16 kg
0.30 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Flexural Yield Strength 28.5 MPa
4130 psi
ASTM D790
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 175 - 205 °C
347 - 401 °F
Users viewing this material also viewed the following: